Making Prussian Blue

Great_Wave_off_Kanagawa (1280x876).jpg

Instructions

A solution of 2 g FeCl3 in 100 ml deionized water is slowly poured into a stirred solution of 1 g K4[Fe(CN)6] in 200 ml deionized water. The blue precipitate is filtered and dried at elevated temperature (c. 100°C)